Ultra high resistance coating

The square resistance is effectively controlled between 5e8 and 5e9 Ω / □, and the film transmittance is more than 98.5%. Various RA tests (such as heat resistance test, high temperature and humidity test, high and low temperature change test, etc.) can be effectively controlled within 10 times.